ISO 11357-5:2013-Plastics — Differential scanning calorimetry (DSC)-Part 5: Determination of characteristic reaction-curve temperatures and times, enthalpy of reaction and degree of conversion

ISO 11357-5:2013

ISO 11357-5:2013-Plastics — Differential scanning calorimetry (DSC)-Part 5: Determination of characteristic reaction-curve temperatures and times, enthalpy of reaction and degree of conversion

Měna
1 800 Kč
Označení normy:ISO 11357-5:2013
Počet stran:10
Vydání:2
Vydáno:2013
Popis

ISO 11357-5:2013


ISO 11357-5:2013 specifies a method for the determination of reaction temperatures and times, enthalpies of reaction, and degrees of conversion using differential scanning calorimetry (DSC). The method applies to monomers, prepolymers, and polymers in the solid or liquid state. The material can contain fillers and/or initiators in the solid or liquid state.