Cena s DPH / bez DPH
Hlavní stránka>ISO 14322:2018 - Plastics — Epoxy resins — Determination of degree of crosslinking of crosslinked epoxy resins by differential scanning calorimetry (DSC)
sklademVydáno: 2018-07-19
ISO 14322:2018 - Plastics — Epoxy resins — Determination of degree of crosslinking of crosslinked epoxy resins by differential scanning calorimetry (DSC)

ISO 14322:2018

ISO 14322:2018 - Plastics — Epoxy resins — Determination of degree of crosslinking of crosslinked epoxy resins by differential scanning calorimetry (DSC)

Formát
Dostupnost
Cena a měna
Anglicky PDF
K okamžitému stažení
Tisknutelné
1916 Kč
Anglicky Tisk
skladem
1916 Kč
Označení normy:ISO 14322:2018
Vydání:2
Vydáno:2018-07-19
Počet stran (Anglicky):8
Popis

ISO 14322:2018

This document specifies a method whereby the heat of reaction generated during epoxy resin crosslinking is measured by differential scanning calorimetry (DSC). The degree of crosslinking is determined based on this result.

This method is applicable to epoxy resin systems with a moderate or slow crosslinking-reaction speed. It might not be applicable to systems with a fast crosslinking-reaction speed at ambient temperature.