Hlavní stránka>ISO 15614-1 Specification and qualification of welding procedures for metallic materials — Welding procedure test — Part 1: Arc and gas welding of steels and arc welding of nickel and nickel alloys — Amendment 2
Not available online - contact us!
sklademVydáno: 2017/FDAmd 2
ISO 15614-1 Specification and qualification of welding procedures for metallic materials — Welding procedure test — Part 1: Arc and gas welding of steels and arc welding of nickel and nickel alloys — Amendment 2

ISO 15614-1

Specification and qualification of welding procedures for metallic materials — Welding procedure test — Part 1: Arc and gas welding of steels and arc welding of nickel and nickel alloys — Amendment 2

Měna
988 Kč
Označení normy:ISO 15614-1
Počet stran:1
Vydání:2
Vydáno:2017/FDAmd 2
Jazyk:Anglicky
Popis

ISO 15614-1