ISO 18177:2025 - Plastics — Test method for estimation of the short chain branching distribution of semicrystalline ethylene 1-olefin copolymers — Differential scanning calorimetry (DSC)

ISO 18177:2025

ISO 18177:2025 - Plastics — Test method for estimation of the short chain branching distribution of semicrystalline ethylene 1-olefin copolymers — Differential scanning calorimetry (DSC)

Formát
Dostupnost
Cena a měna
Anglicky PDF
K okamžitému stažení
Tisknutelné
3861 Kč
Anglicky Tisk
skladem
3861 Kč
Označení normy:ISO 18177:2025
Vydání:1
Vydáno:2025-05-13
Počet stran (Anglicky):20
Popis

ISO 18177:2025

This document specifies a test method for the estimation of the short chain branching distribution of semicrystalline ethylene 1-olefin copolymers by successive self-nucleation and annealing (SSA) with conventional, high performance and fast differential scanning calorimetry.

This document is applicable to the estimation of the short chain branching distribution of raw materials of semicrystalline ethylene 1-olefin copolymers and its products.

Quantitative calculation of short chain branching content, degree of crystallinity and short chain branching distribution is applicable to ethylene/1-butene copolymers, ethylene/1-hexene copolymers and ethylene/1-octene copolymers.