Hlavní stránka>ISO 14373:2024 - Resistance welding — Procedure for spot welding of uncoated and coated low-carbon steels
sklademVydáno: 2024-01-22
ISO 14373:2024 - Resistance welding — Procedure for spot welding of uncoated and coated low-carbon steels

ISO 14373:2024

ISO 14373:2024 - Resistance welding — Procedure for spot welding of uncoated and coated low-carbon steels

Formát
Dostupnost
Cena a měna
Anglicky PDF
K okamžitému stažení
Tisknutelné
2860 Kč
Francouzsky PDF
K okamžitému stažení
Tisknutelné
2860 Kč
Anglicky Tisk
Skladem
2860 Kč
Francouzsky Tisk
Skladem
2860 Kč
Označení normy:ISO 14373:2024
Vydání:3
Vydáno:2024-01-22
Počet stran (Anglicky):14
Počet stran (Francouzsky):16
Popis

ISO 14373:2024

This document specifies requirements for resistance spot welding in the fabrication of assemblies of uncoated and metallic-coated or weldable non-metallic-coated low-carbon steel, comprising two or three sheets of metal, where the maximum single-sheet thickness of components to be welded is within the range 0,4 mm to 3,0 mm.

This document is applicable to welding of sheets of the same or unequal thickness, where the thickness ratio is less than or equal to 3:1.

Welding with the following types of equipment is within the scope of this document:

a)       pedestal welding equipment;

b)       portable welding guns;

c)        automatic welding equipment where the components are fed by robots or automatic feeding equipment;

d)       multi-spot-welding machines;

e)       robotic welding machines.